Putty (white) for exterior walls
RETURN
The product is made of imported materials, high-quality cement and fine fillers. It has the characteristics of high strength and good flexibility, and can fully play the role of leveling and decoration of exterior walls.
  • Product advantage

    1. It has a high bonding strength.

    2. It has good flexibility and can resist the shrinkage caused by thermal expansion and contraction of the base course.

    3. It has a high whiteness and helps to improve the covering capacity of the paint.

  • Product parameter

    1. It is used to repair and reinforce the cracks in bathroom, kitchen, basement, swimming pool and other parts.

    2. It is used to repair and reinforce the defects of all kinds of wall-piercing pipes, bushings, and other parts around the pipe mouth.

    3. It is used for repairing and strengthening node parts such as canal root and Yin and Yang Angle.

  • Construction process

     

     

    Step One:“Base course treatment”

    The base course shall be solid, clean and roughly flat; the PH value shall be less than 10, and the water content shall be less than 10%; if the base course has a high water absorption rate, it shall be wetted with clear water or treated with an interface agent in advance.

     

    Step Two:“Adding water and mixing”

    Pour water into the bucket (the mass ratio of putty to clear water is about 100:33~36), and add the powder material while mixing. The mixing time shall be 5-8 minutes, mixing shall be stopped for 2 minutes, and then the second mixing shall be carried out for 2 minutes before use.

     

    Step Three: “Applying the mixed adhesive

    The second layer shall be applied until the first layer is completely dry, and the time interval shall be ≥ 4h in summer and ≥ 24h in winter. (Actually, it varies due to the local climate and the coating thickness of putty during construction).

     

    Step Four:“Wall grinding”

    After the construction is completed, it can be carefully ground with sand paper or a wall grinding machine.

  • Notes

    ✔ The temperature on the construction site shall be between 5°C and 35°C.

    ✔ Avoid applying it at the same time of applying the polyester paint.

    ✔ The second layer shall be applied until the first layer is completely dry, and the time interval shall be ≥ 24h.

    ✔ Don't use too thick sandpaper when sanding. It is recommended that the fineness of sand paper should be between 600 and 1000 meshes.